Chemical composition %
C | Si | Mn | S | Ni | Fe | Other |
≤2.00 | ≤2.50 | ≤1.80 | ≤0.03 | 45-60 | Remainder | ≤1.00 |
Reference current
mm | 3.2 | 4.0 | 5.0 | |
A | 90-100 | 120-150 | 160-190 |
Z408Nickel ferroalloy welding core, strong reducing graphite cast iron welding type medicine leather, high strength, good, first developed low expansion coefficient, the anti-cracking characteristics of gray iron and z308 almost
But for ball mill cast iron is strong, z308 to the phosphorous higher cast iron, also have good effect, machinability is a bit poor, than z308 for normal temperature or slightly preheat (200 degrees Celsius) or so, gray iron and ball mill iron welding, ac/dc amphibious, arc stability, convenient operation.
NOTE
Before welding electrode in 150 degrees Celsius must be approved by a baking 1 hour
Cast iron welding rod CD-Z408