1. PVD coating.
2. Coating material: TiAIN
3. Coating Microhardness: HV3200.
4. Coating temperature: 450-480 degree centigrade, without effect on ultra-grained alloy substrate.
5. Coating failure temperature: 900 degree centigrade, high heat resistance.
6. Gurantee the sharp cutting edge after coating.
7. Can manufacture different grades for milling different metals, such as steel, stainless steel, cast iron, and aluminum.
8. Excellent quality, fast delivery time, and competitive price.