Ads by Google
Stainless Steel 314 Bar
The best high-temperature resistance capabilities of any chromium-nickel steels can be found in Stainless 314. Silicon improves oxidation and carburization resistance, but may make more brittle when subjected to lengthy temperatures of 1200° to 1500°F (649° to 816°C).
Chemical Composition
Element | Weight % |
C | 0.25 |
Mn | 2.00 |
Si | 1.5-3.0 |
Cr | 23.0-26.0 |
Ni | 19.0-22.0 |
P | 0.045 |
S | 0.03 |
Mechanical Properties
Properties | Conditions | ||
T (°C) | Treatment | ||
Density (×1000 kg/m3) | 7.8 | 25 | |
Poisson's Ratio | 0.27-0.30 | 25 | |
Elastic Modulus (GPa) | 200 | 25 | |
Tensile Strength (Mpa) | 515 | 25 | hot finished and annealed (wire) |
Yield Strength (Mpa) | 205 | ||
Elongation (%) | 40 | ||
Reduction in Area (%) | 50 |
Thermal Properties
Properties | Conditions | ||
T (°C) | Treatment | ||
Thermal Expansion (10-6/ºC) | 15.1 | 0-315 | |
Thermal Conductivity (W/m-K) | 17.5 | 100 | |
Specific Heat (J/kg-K) | 500 | 0-100 |
Electric Properties
Properties | Conditions | ||
T (°C) | Treatment | ||
Electric Resistivity (10-9W-m) | 770 | 25 |
973-276-5000f: 973-276-5050 toll free: 800-600-9290HomeWarehouse ProductsForgingsCustom Hand-Rolled BarsCustom MeltingValue Added ServicesFree CatalogQuick LiteratureIn the NewsWhite PapersMetals OutlookSend Request for QuoteAlloy Information Report for Stainless Steel 314Request for QuoteGeneral Characteristics of Stainless 314
The best high-temperature resistance capabilities of any chromium-nickel steels can be found in Stainless 314. Silicon improves oxidation and carburization resistance, but may make more brittle when subjected to lengthy temperatures of 1200° to 1500°F (649° to 816°C).