high speed steel M42(W2Mo9Cr4VCo8)
Anneal temperature: 860-880
Relief annealing temperature: 720-760
Hardening temperature: 1160-1190
Hardening medium: salt bath under 600,aslo use oil cooling or air cooling
Normal temper temperature: 540-560RC Rockwell Hardness after hardening and temper: 66-68
Characteristic:High performance tungsten-molybdenum high speed steel, Excellent performance of hardness, red hardness, thermoplasticity, machinability. Only weak in toughness
Application: used in various of complicated tools,e.g pricision broaches, form cutter,professional lathe tool and various high hardness tools.