ukraine reinforcing steel bar 1. Important building material 2. Welcome OEM 3. Make new moulds for you

45# 50/55/60/65/90 ukraine reinforcing steel bar

Material

C

Si

Mn

P≤

S≤

Ni

Cr

Mo

Cu

45#

0.42-0.50

0.17-0.35

0.50-0.80

0.030

0.030

0.25

0.25

 

0.20

27SiMn

0.24-0.32

1.10-1.40

1.10-1.40

0.030

0.030

0.30

0.30

 

0.30

40Cr

0.37-0.44

0.17-0.35

0.50-0.80

0.030

0.030

0.30

0.80-1.10

 

0.25

20CrMnTi

0.17-0.23

0.17-0.37

0.80-1.10

0.035

0.035

0.30

1.0-1.30

 

0.30

42CrMo

0.38-0.45

0.17-0.35

0.50-0.70

0.030

0.030

0.3

0.80-1.10

0.15-0.25

0.20

16Mn

≤0.20

≤0.55

1.00-1.60

0.035

0.035

    

27SiMn

0.24-0.32

1.10-1.40

1.10-1.40

0.030

0.030

0.30

0.30

 

0.30

Grade

GB Q255/JIS SS490/DIN S275J0/ASTM 1025

Standard

GB,JIS,ASTM,DIN,AISI,BS

Size

carbon steel      Width: 500mm-3300mm                          Length:7000mm-12000mm

carbon steel round bar: diameter 18-300mm

Surface treatment

as your requirement

Inspecting

UTS according to SEP1921 C/c or GB/T6402

Quality Control

test products mechanical and chemical properties in every procedure(third party inspection institution: CIQ, SGS, ITS, BV, etc)

Delivery State

Hot forged, Black &Annealing

Hardness

HBS=137~269

Characteristic Application

welding is well, Used for making normal machinery parts, such as bolt, chain, pull rod, shape steel, steel plate, flat bar steel and so on

Packaging 

We provide the package according to the export standard or as client's requirements.

Delivery Time

within 30 days after we receive the deposit

Material

42CrMo/45#/40Cr/20CrMnTi/27SiMn/16Mn

Isothermal annealing:

Heat to 850°Chold for 1/2 hour to 1 hour;

Furnace cooling to 770°C and hold at temperature for at least 10 hours;

Cool by 10°C /h to 720°C;

Cooling in air.

Stress relieving:

To be carried out after machining and before the final heat treatment.

Heat to 650-700°C, hold for 4/6 hours:

Furnace cooling to 330-350°C;

Cooling in air.

Hardening:

Initial preheating to 350-450°C;

Second preheating to 750-850°Cin salt bath at 850°C;

Austenitizing at 960-100°C;

Cooling in fluid oil.

( function(){ var aBigImageSrc = [ 'http://i01.i.aliimg.com/photo/v0/829750881_1/45_carbon_round_ukraine_reinforcing_steel_bar.jpg' , 'http://i01.i.aliimg.com/photo/v0/829750881_2/45_carbon_round_ukraine_reinforcing_steel_bar.jpg' , 'http://i01.i.aliimg.com/photo/v0/829750881_3/45_carbon_round_ukraine_reinforcing_steel_bar.jpg' , 'http://i01.i.aliimg.com/photo/v0/829750881_4/45_carbon_round_ukraine_reinforcing_steel_bar.jpg' , 'http://i01.i.aliimg.com/photo/v0/829750881_5/45_carbon_round_ukraine_reinforcing_steel_bar.jpg' , 'http://i01.i.aliimg.com/photo/v0/829750881_6/45_carbon_round_ukraine_reinforcing_steel_bar.jpg' ]; var oProductShow = new AE.run.minisite.productShow(); oProductShow.init( { 'aImgSrc': aBigImageSrc } ); } )(); 45# carbon round ukraine reinforcing steel bar

Ads by Google

Hot Products: A | B | C | D | E | F | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z | 0-9
Copyright Notice @ 2008-2022 ECOL Limited and/or its subsidiaries and licensors. All rights reserved.