Superalloy

Aug 24, 2012
Superalloy
(Heat-resisting Superalloy Anticorrosion Alloy) Forged bar Size: 50-305mm Application: nuclear energy, ... acid, phosphoric acid, acetic acid, and other industries.(Heat-resisting Superalloy Anticorrosion Alloy) Hot-rolled barGrade: 10-85mmApplication: aviation, spaceflight, nuclear ... :Competitive price Good quality Timely delivery Perfect after-sales service Superalloy
Supplier: HY (Shanghai) Industry Co., Ltd. [China Manufacturers]
Nickel-based alloy forgings
Nickel-based alloy forgings Nickel Alloy Butt Weld & Forged FittingGrade: UNS 2200 (NICKEL 200), UNS 4400 (MONEL 400), UNS 8825 INCONEL (825 ), UNS 6600(INCONEL 600), UNS 6601 (INCONEL 601), UNS 6625 (INCONEL 625), UNS 10276 (HASTELLOY C 276), UNS 2201 (NICKEL 201), (ALLOY 20 / 20 CB 3)
Supplier: Baoji City Hengxin Rare Metal Co., Ltd. [China Manufacturers]

OEM Upset Spindle

Mar 27, 2012
OEM Upset Spindle
... axle; as OEM we can supply forged and machined parts; Upset Spindle equipped with total 39 forging production lines consisted of ... advantages in developing and producing high-tech, accurate and large forgings. And toolings with high accuracy can also be achieved by ...

aluminum forgings

Mar 31, 2013
aluminum forgings
... . -excellent surface treatment technique for aluminum forgings aluminum part include: alodine, anodizing, powder coating, polishing, Nickel plate, chromate plating, zinc plating, gold ... finish, e-coating, wet painting, passivation and etc. Here below are some aluminum forgings material ...
Supplier: Ningbo Yinzhou Intime Machinery Co., Ltd. [China Manufacturers]
Monel alloy 400/N04400/2.4360 superalloy wire rod
... aminate conditions corrosion below 585 °C due to the high nickel.Monel 400 Application fieldMonel 400 alloy is a multi-purpose ... Width700-1000 m/m Monel alloy 400/N04400/2.4360 superalloy wire rod
Supplier: Hlmet Co., Ltd. [China Manufacturers]
superalloy wire,superalloy bar
... shape products,like superalloy bar,superalloy rod,superalloy wire,superalloy ingot,superalloy strip,superalloy plate,superalloy tube,etc. Superalloy is one of ... foreign companies. Our goal is to produce superalloy materials of specification and designation needed by customers ... alloy and powder alloy. The main requirements of superalloy properties are heat-stability, heat-strength and texture ...
Supplier: AT&M International Trading Co., Ltd. [China Manufacturers]
Nickel Alloy Inconel 625 Plate
... Plate 1.nonmagnetic, corrosion and oxidation resistant, nickel-base alloy 2.Ni:58% min Nickel Alloy Inconel 625 PlateWe produce this grade ... in the following forms: Bar, wire, sheet, plate, coil, fasteners and forgings.INCONEL ... strength(mpa)Yield strength(mpa)Elongation in 50 mm(%)83041030 Nickel Alloy Inconel 625 Plate
Supplier: Tianjin Haozeshun Trade Co., Ltd. [China Manufacturers]

forgings

Jun 17, 2012
forgings
... -Cobalt, controlled expansion alloy containing 29% Nickel. It's coefficient of expansion we produce the products with ... , welded pipe, seamless tube, welded tube, bar, wire, sheet, plate, forgings, pipe fittings and flanges,strip ...
Supplier: Shanghai Fengqu Super Alloy Co., Ltd. [China Manufacturers]
Hastelloy G-30/N06030/Alloy G30 corrosion-resisting superalloy wires
... diameter:8-2000mm. 2.plate/sheet thickness:2-200mm. 3.forgings weight:0.5-10000Kg. 4.pipe/tube OD80-3500mm. 1 ... 2.Description HASTELLOY G-30 alloy is a high chromium nickel-base alloy which shows superior corrosion resistance over most other ... nickel- and iron-base alloys in commercial phosphoric acids as well ...

forgings 2

Mar 04, 2012
forgings 2
As forging parts, O.E.M. welcome. forgings 2
22% min Nickel Sulphate (Nickelous sulfate)
... .05maxCu0.002 max0.005 maxPb0.002 max0.005 maxApplication: Electroplating, nickel-cadmium battery, organic synthesis, catalyst in painting production, raw material ... of nickel salt for coloring of metals and additives of reduction dye ... with double plastic bags lined plastic woven bag. 22% min Nickel Sulphate (Nickelous sulfate)
Supplier: Lubon Industry Co., Ltd. [China Manufacturers]

Nickel oxide

Dec 10, 2012
Nickel oxide
Nickel oxide Appearance: green powder usage: glass industrial, other industrial F. ... ,borax, cobalt oxide, potassium carbonate, etc. Detailed Product Description Product: Nickel OxideSpecs.:NiO 76% min.Co 0.03% max.Fe 0 ... meshPacking: 25kgs net Iron drumUsed for glass and ceramic industrials. Nickel oxide
Supplier: Xiangtan New Sunshine Trade Co., Ltd. [China Manufacturers]
brass pipe fitting--nickel plated Tee equal
... Tee equal(ZTN-0111)1.Material:brass 2.Nickel plated 3.CE&ISO9001 4.Sizes:16*16*16 ... -32*32*32 brass pipe fitting--nickel plated Tee equal(ZTN-0111)1.Compay introductionYuhuan Tiannian ... cooperate with us. 2.Product name:brass pipe fitting--nickel plated Tee equal(ZTN-0111)3.FeatureItem no.ZTN-0111Material ... Offered4.Sizes 5.Following customers' design brass pipe fitting--nickel plated Tee equal
Supplier: Yuhuan Tiannian Valve Co., Ltd. [China Manufacturers]
Lever Handle Nickel Plated Brass Water Bibcock FW-C1018
... Bibcock 1,Body Material: brass or Zamak 2,Surface:Nickel Plated Lever Handle Nickel Plated Brass Water Bibcock 1, body material: brass ... accessories,with good quality and pretty competitive price. Lever Handle Nickel Plated Brass Water Bibcock FW-C1018
Supplier: Yuhuan Forus Sanitary Ware Co., Ltd. (Well Way) [China Manufacturers]
nickel brass equal tee
... walls result in low pressure loss and high volumePackage: carton nickel brass equal tee
Supplier: Zhejiang Newkeli Piping Systems Co., Ltd. [China Manufacturers]
Gas Ball Valve with Nickel Plating
... connector, barb hose connector.5. Surface: Yellow brass color, or Nickel plated, or Chrome plated.6. Certification: ISO9001:2000.7. OEM ... to contact us for more information. Gas Ball Valve with Nickel Plating
Supplier: Changshan Hongfeng Tubing Co., Ltd. [China Manufacturers]
Nickel Plating bolts
... :Self Color,Black,Teflon Coating(PTFE) Black, White,Blueness Zinc,Nickel Plating 3.MS,CS,SS Stud Bolts & Nuts Size 1 ... Zinc (Cr.3 or Cr.6), Dacromet, Hot Dip Galv, Nickel Plating .Packing: CARTON/PALLET ,Standard packing or According to customers ...
Supplier: Weifang Shengjiang Import & Export Co., Ltd. [China Manufacturers]
Bibcocks Brass Bibcock Nickel Size:1/2"
1.Product : Brass Bibcock Nickel 2. Bibcock 3.Size: 1/2" 1.Product : Brass Bibcock Nickel 2. Bibcock 3.Size: 1/2" 4. Material: brass 5. Advantage : Good quality competitive price and good service 6. Use : Building Material Plumbing Material Bibcocks Brass Bibcock Nickel Size:1/2"
Supplier: Ningbo Tieda Import & Export Co., Ltd. [China Manufacturers]

Customized forgings

Jun 08, 2012
Customized forgings
customized forgings and machined parts for pressure equipment and pipe engineering. we ... varieties of high-pressure pipe fittings and mechanical parts. Customized forgings
Supplier: Shaanxi Fenry Flanges And Fittings Co., Ltd. [China Manufacturers]
Ads by Google


Hot Products: A | B | C | D | E | F | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z | 0-9
Copyright Notice @ 2008-2022 ECOL Limited and/or its subsidiaries and licensors. All rights reserved.