Typical Properties:
Item | Unit | Typical Value | Test Method | |
Membrane Thickness | μm | 22 | ASTM D-374 | |
Tensile Strength | MD | Mpa | 130 | ASTM D-882 |
TD | 268 | |||
Elongation At Break | MD | % | 165 | ASTM D-882 |
TD | 50 | |||
Thermal Shrinkage (120,2min | MD | % | 3.8 | ASTM D-1204 |
TD | 1.2 | |||
Hot Sealing Property | N/15mm | 4.2 | ASTM D-882 | |
Wetting Tension | mN/m | 40 | ASTM D-2578 | |
Friction Coefficient(For Bare Film) | 0.35 | ASTM D-1894 | ||
Haze(For Bare Film) | % | 0.9 | ASTM D-1003 | |
Gloss(For Bare Film) | % |
| ASTM D-2457 | |
Aluminum Thickness | A | 380 |
| |
Ω/ | 1.53 | GB/T 15717 | ||
O.D | 2 | X·Rite361 | ||
(Light Transmission) VLT
|
| ASTM D 1746 | ||
Aluminum Uniformity | % | 8.2 |
| |
Adhesion of Aluminum Layer | % | Aluminum peel2 | 3M Tape |