Standard :GB 4948
used for Hull, Ballast tanks, offshore engineering, Harbor Structures, Sea water cooling system,etc
Aluminum anodes. Which can be used for Hull, Ballast tanks, offshore engineering, Harbor Structures, Sea water cooling system, and submerged pipelines.
Standard :GB 4948Chemical Composition Analysis (%) Type | Zn | In | Cd | Sn | Mg | Si | Ti | Impurity ,less than | Al | Si | Fe | Cu | Al-Zn-In-CdA11 | 2.5-4.5 | 0.018-0.050 | 0.005-0.020 | - | - | -- | - | 0.10 | 0.15 | 0.01 | Balance | Al-Zn-In-SnA12 | 2.2-5.2 | 0.020-0.045 | - | 0.018-0.035 | - | - | - | 0.10 | 0.15 | 0.01 | Balance | Al-Zn-In-SiA13 | 5.5-7.0 | 0.025-0.035 | - | - | - | 0.10-0.15 | - | 0.10 | 0.15 | 0.01 | Balance | Al-Zn-In-Sn-MgA14 | 2.5-4.0 | 0.020-0.050 | - | 0.025-0.075 | 0.50-1.00 | - | - | 0.10 | 0.15 | 0.01 | Balance | Al-Zn-In-Mg-TiA21 | 4.0-7.0 | 0.02-0.050 | - | - | 0.50-1.50 | - | 0.01-0.08 | 0.10 | 0.15 | 0.01 | Balance | Electrochemical characteristics : Item | Material of anodes | Open-circuit Voltage (v) | Close-circuit Voltage (v) | Actual Capacity(Ah/kg) | Current efficiency (%) | Consumption rate ( kg.(A.a)* | Dissolve Performance | Electrochemical Performance | Type 1 | -1.18- -1.10 | -1.12- -1.05 | ≥2400 | ≥85 | ≤3.65 | The surface dissolve evenly & oxide drop easily | Type 2 | -1.18- -1.10 | -1.12- -1.05 | ≥2600 | ≥90 | ≤3.37 | *Reference electrode: Saturated calomel electrode Type 1: A11,A12,A13,A14 Type 2: A21 |
|
Aluminium anode