Welcome to ECOL - Join Free - Sign In
welding flux
welding flux
Supplier Info
[China Supplier]
Contact Person : Ms. Zhang Sophia
Tel : 86-575-86110998
Fax : 86-575-86110998
Product Detail
1.Material: CuO2,Al 2. high efficiency and safe 3. simple operation 4.OEM service available

Exothermic welding is a simple, high efficiency and high quality method of metal connecting.

Lihe exothermic welding is a high temperature reaction of powdered copper oxide and aluminum. The chemical equation is 2Cu2O+2Al=6Cu+Al2O3 ( the temperature can be in excess of 2500°C.) It is a method of welding copper, iron, steel and ferroalloy without outside power.

In order to weld different sizes conductor, a graphite mold is needed. It is only to put the conductor need welding in the mold, dump powder into the mold, ignite the starting powder, than the reaction takes place. Open the mold when it is cold, thus the conductor connection is finished. We supply different connections and the matched mold and welding powder.

Characteristics

Good current loading ability

The welding point current loading ability is the same as conductor.

Good mechanical performance

The connection is a molecular connection. It is a permanent connection.

Stable dash current resistance

The test shows that in the surge of big current in short time, the conductor melts earlier than the connection point, so it will not be damaged by surge current.

Good resistance to corrosion

The welding point is covered by copper, it provides good resistance to corrosion.

Simple and safe connection

Neither outside power nor facility is required. It requires very little time to finish one welding. It can be done both indoor and outdoor.

Free control the reaction temperature

Different welding powder is provided according to the metal features, so the welding powder can be very solid.

Making a exothermic welding connection

Make sure the mold is dry, by pre-heating, put the cleaned conductors in mold.Place metal disc in bottom of mold crucible and close the mold.Dump welding powder into crucible, and place starting powder in the ignition pocket.Close lid, ignite the starting powder with the flint gun.Reaction takes place in the graphite mold.Open the lid when it is cold. The welding connection is done.

welding flux

Verified Information This information is Verified by TÜV Rheinland and is valid for the following period: 2013/01/17 --- 2014/01/17 All the information below may covers both Gold Supplier and its related companies , Their Relationship will be affirmed according to china laws and regulations , also it will be clearly display in the full report >> Production Capacity: Product line name Production Line Capacity Actual Units Produced(Previous Year)
Copper Bonded Earth Rod and Accessories Copper Bonded Earth Rod 100,000 Pieces / Month, Copper Bonded Earth Rod Accessories 200,000 Pieces / Month Copper Bonded Earth Rod 1,000,000 Pieces, Copper Bonded Earth Rod Accessories 2,000,000 Pieces
Export Market Distribution: Market Revenue(Previous Year) Total Revenue (%)
North America USD 400,000 25.48
Southeast Asia USD 80,000 5.1
Africa USD 240,000 15.29
Western Europe USD 20,000 1.27
Central America USD 30,000 1.91
Domestic Market USD 800,000 50.95
Production Machinery: Machine Name Brand & Model No. Quantity Number of Year(s) Used Condition
Cutting Machine No Information 1 2.0 Acceptable
Lathe CJ035 4 2.0 Acceptable
Punching Machine J23-16 1 2.0 Acceptable
Thread Rolling Machine Z28-80 1 2.0 Acceptable
Electroplating Production Line No Information 1 2.0 Acceptable
Drilling Machine Xiling 2 2.0 Acceptable
Testing Machinery: Machine Name Brand & Model No. Quantity Number of Year(s) Used Condition
Copper Layer Thickness Tester PosiTector 2 2.0 Acceptable
Production Flow: 1.Cutting 2.Lathing 3.Thread Rolling 4.Punching 5.Drilling 6.Electroplating
Ads by Google

Hot Products: A | B | C | D | E | F | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z | 0-9
Copyright Notice @ 2008-2022 ECOL Limited and/or its subsidiaries and licensors. All rights reserved.