Silicone Rubber Glassfiber insulating Sleeving(inside fiber and outside rubber)is braided into tubes with non-alkali glassfiber,and then painted with silicone rubber through high temperature.It has better features than silicone glassfiber tubes in the aspect of electricity-avoidness,flame off-self and flexibility.It is widely used in insulating protection of H&N Grade automobile,shipbuiding,electrical machinery,home appliance,electric&heat equipment,special lightware.etc.
Technology index off-self time: 30 seconds
Type/file No. | Testing Condition | Lighting-resistance | Temperature-resistunce | Average voltage | Individual Value |
SGS-40 E233804 | UL1441 | UL V W-1 | +200°C-10°C | 4000V | 3000V |
SRS-70 E233803 | UL1441 | UL V W-1 | +200°C-10°C | 7000V | 5000V |
Inside diameter measurement
Inside diameter | Wall thickness | ||
Range | Tolerance | 4000V | 7000V |
0.5-2.0mm | +0.20-0.00mm | 0.40mm±0.05mm | 0.45±0.05mm |
2.5-3.0mm | +0.25-0.00mm | 0.40mm±0.05mm | 0.50±0.05mm |
3.5-5.0mm | +0.35-0.00mm | 0.45mm±0.05mm | 0.55±0.05mm |
6.0-9.0mm | +0.50-0.00mm | 0.50mm±0.05mm | 0.60±0.05mm |
10.0-12.0mm | +0.70-0.00mm | 0.60mm±0.05mm | 0.65±0.05mm |
Specification
ITEM | VALUE |
Continuous Operating Temperature | -10°C+200°C |
Temperature Endurance | 265°C±2°C 168>1/2 Original value of voltage |
Aging Test | 260°C, 6 hrs without crackle |
Cold Bend | Without crackle |
Horizontal Flame Test | <30 seconds |
(V W-1)Flame Retardance | <30 seconds |
Submerge Water Test | Not-sticky,non-deformed,non-bated |