Post-processed Glass Fibre Fabric features good electric insulation,corrosion-resistance and high intensity.
The content of alkai mental oxide is within 0.8%.
Size residue of paraffin emulsion is not more than 0.18%.
coupling agent content in KH550/560 processed fabric is not lower than 0.10%.
whiteness of EW140 and EW100 is not less than 80.
Whiteness of EW200 is not less than 70.
Usage
This produce is suitable to be used as the base material of printed circuit board anf insulating laminate. Base material For PCB.
Product list
Product type | Tickness (mm) | Width(cm) | Weight (g/m2) | Breaking Strength no less than N/a strip of cloth 25×100mm Warp Weft | Weave | Application | |
EW100 | 0.10±0.01 | 90--127 | 100±10 | 157 | 157 | plain | Base material for PCB |
EW140 | 0.14±0.014 | 136±14 | 200 | 180 | plain | ||
EW200 | 0.20±0.02 | 203±20 | 300 | 230 | plain |
Special products and other specifications are according to customers requirements .