The rolls are to be used at Recersible Mill and Temper Mill
high quality with quick lead time;
widely used in steel mill
C : 0.70-0.80%Si : 0.20-0.60%Mn : 0.15-0.45%Ni : 0.30% maxCr : 1.40-1.70%Mo : 0.20-0.30%P : 0.04% maxS : 0.04% max MAT . 75XMWT : 30000KGBarrel dia 1400+0.50 MMDiscard dia 1320MMHardness:a) Barrel 55-75 shore C ( It should be less than HS 55 C at discarded diameter)b) Journal 33-60 shore CDepth of hard shell of Roll barrel 45mmTensile Strength 120kgf/mm2 minElongation 3% min